title={The Optimum Addition Ratio of Nano Hydroxyapatite to Glass Ionomer Dental Cement (Changes in Demineralization Resistance and Bonding Strength of Light Cured Glass Ionomer after the Addition of Nano Hydroxyapatite in Various Ratio)},
journal={Journal of the Korean academy of pediatric dentistry},
issn={1226-8496},
year={2013},
volume={40},
number={3},
pages={159-167},
doi={10.5933/JKAPD.2013.40.3.159}
TY - JOUR
AU - 김남혁
AU - SEONG OH KIM
AU - Je Seon Song
AU - JAE HO LEE
AU - Heung Kyu Son
AU - Byungjai Choi
AU - HYUNG JUN CHOI
TI - The Optimum Addition Ratio of Nano Hydroxyapatite to Glass Ionomer Dental Cement (Changes in Demineralization Resistance and Bonding Strength of Light Cured Glass Ionomer after the Addition of Nano Hydroxyapatite in Various Ratio)
JO - Journal of the Korean academy of pediatric dentistry
PY - 2013
VL - 40
IS - 3
PB - The Korean Academy Of Pediatric Dentistry
SP - 159
EP - 167
SN - 1226-8496
AB - The aim of this study was to evaluate changes in demineralization resistance and bonding strength of light cured glass ionomer after the addition of nano hydroxyapatite in various ratios. Fuji II LC GIC (GC Co., Japan)was used as the control group and also as a base material for experimental group. HA was mixed into the RMGIC at various ratio to create a HA-LC GIC mixture, preparing six experimental groups, i.e. 5%, 10%, 15%,20%, 25%, 30% HA-LC GIC. According to the results, the bonding strength increased due to the addition of HA, showing the maximum value at the 15% nano HA group (p < 0.05). Under CLSM observation after 4 days of demineralization, the HA groups were more resistant to demineralization compared to the control group. No significant difference was observed between HA groups. In analysis through SEM, the HA groups showed attachment of granular materials and decreased demineralized tooth surfaces under influence of HA particles.
KW - Nano hydroxyapatite;Light-cured glass ionomer;Bonding strength;Demineralization resistance
DO - 10.5933/JKAPD.2013.40.3.159
ER -
김남혁, SEONG OH KIM, Je Seon Song, JAE HO LEE, Heung Kyu Son, Byungjai Choi and HYUNG JUN CHOI. (2013). The Optimum Addition Ratio of Nano Hydroxyapatite to Glass Ionomer Dental Cement (Changes in Demineralization Resistance and Bonding Strength of Light Cured Glass Ionomer after the Addition of Nano Hydroxyapatite in Various Ratio). Journal of the Korean academy of pediatric dentistry, 40(3), 159-167.
김남혁, SEONG OH KIM, Je Seon Song, JAE HO LEE, Heung Kyu Son, Byungjai Choi and HYUNG JUN CHOI. 2013, "The Optimum Addition Ratio of Nano Hydroxyapatite to Glass Ionomer Dental Cement (Changes in Demineralization Resistance and Bonding Strength of Light Cured Glass Ionomer after the Addition of Nano Hydroxyapatite in Various Ratio)", Journal of the Korean academy of pediatric dentistry, vol.40, no.3 pp.159-167. Available from: doi:10.5933/JKAPD.2013.40.3.159
김남혁, SEONG OH KIM, Je Seon Song, JAE HO LEE, Heung Kyu Son, Byungjai Choi, HYUNG JUN CHOI "The Optimum Addition Ratio of Nano Hydroxyapatite to Glass Ionomer Dental Cement (Changes in Demineralization Resistance and Bonding Strength of Light Cured Glass Ionomer after the Addition of Nano Hydroxyapatite in Various Ratio)" Journal of the Korean academy of pediatric dentistry 40.3 pp.159-167 (2013) : 159.
김남혁, SEONG OH KIM, Je Seon Song, JAE HO LEE, Heung Kyu Son, Byungjai Choi, HYUNG JUN CHOI. The Optimum Addition Ratio of Nano Hydroxyapatite to Glass Ionomer Dental Cement (Changes in Demineralization Resistance and Bonding Strength of Light Cured Glass Ionomer after the Addition of Nano Hydroxyapatite in Various Ratio). 2013; 40(3), 159-167. Available from: doi:10.5933/JKAPD.2013.40.3.159
김남혁, SEONG OH KIM, Je Seon Song, JAE HO LEE, Heung Kyu Son, Byungjai Choi and HYUNG JUN CHOI. "The Optimum Addition Ratio of Nano Hydroxyapatite to Glass Ionomer Dental Cement (Changes in Demineralization Resistance and Bonding Strength of Light Cured Glass Ionomer after the Addition of Nano Hydroxyapatite in Various Ratio)" Journal of the Korean academy of pediatric dentistry 40, no.3 (2013) : 159-167.doi: 10.5933/JKAPD.2013.40.3.159
김남혁; SEONG OH KIM; Je Seon Song; JAE HO LEE; Heung Kyu Son; Byungjai Choi; HYUNG JUN CHOI. The Optimum Addition Ratio of Nano Hydroxyapatite to Glass Ionomer Dental Cement (Changes in Demineralization Resistance and Bonding Strength of Light Cured Glass Ionomer after the Addition of Nano Hydroxyapatite in Various Ratio). Journal of the Korean academy of pediatric dentistry, 40(3), 159-167. doi: 10.5933/JKAPD.2013.40.3.159
김남혁; SEONG OH KIM; Je Seon Song; JAE HO LEE; Heung Kyu Son; Byungjai Choi; HYUNG JUN CHOI. The Optimum Addition Ratio of Nano Hydroxyapatite to Glass Ionomer Dental Cement (Changes in Demineralization Resistance and Bonding Strength of Light Cured Glass Ionomer after the Addition of Nano Hydroxyapatite in Various Ratio). Journal of the Korean academy of pediatric dentistry. 2013; 40(3) 159-167. doi: 10.5933/JKAPD.2013.40.3.159
김남혁, SEONG OH KIM, Je Seon Song, JAE HO LEE, Heung Kyu Son, Byungjai Choi, HYUNG JUN CHOI. The Optimum Addition Ratio of Nano Hydroxyapatite to Glass Ionomer Dental Cement (Changes in Demineralization Resistance and Bonding Strength of Light Cured Glass Ionomer after the Addition of Nano Hydroxyapatite in Various Ratio). 2013; 40(3), 159-167. Available from: doi:10.5933/JKAPD.2013.40.3.159
김남혁, SEONG OH KIM, Je Seon Song, JAE HO LEE, Heung Kyu Son, Byungjai Choi and HYUNG JUN CHOI. "The Optimum Addition Ratio of Nano Hydroxyapatite to Glass Ionomer Dental Cement (Changes in Demineralization Resistance and Bonding Strength of Light Cured Glass Ionomer after the Addition of Nano Hydroxyapatite in Various Ratio)" Journal of the Korean academy of pediatric dentistry 40, no.3 (2013) : 159-167.doi: 10.5933/JKAPD.2013.40.3.159