@article{ART001670866},
author={김한기 and Namsik Yoon and Manwoo Huh and 김익수},
title={Physicochemical Properties of Non-Formaldehyde Resin Finished Cotton Fabric and their Optimal Treatment Condition},
journal={Textile Coloration and Finishing },
issn={1229-0033},
year={2012},
volume={24},
number={2},
pages={121-130},
doi={10.5764/TCF.2012.24.2.121}
TY - JOUR
AU - 김한기
AU - Namsik Yoon
AU - Manwoo Huh
AU - 김익수
TI - Physicochemical Properties of Non-Formaldehyde Resin Finished Cotton Fabric and their Optimal Treatment Condition
JO - Textile Coloration and Finishing
PY - 2012
VL - 24
IS - 2
PB - The Korean Society Of Dyers And Finishers
SP - 121
EP - 130
SN - 1229-0033
AB - Cotton fabrics were treated with some commercial non-formaldehyde and low-formaldehyde resins, and then their effect on the physicochemical properties were respectively investigated including formaldehyde release, tear strength, shrinkage,and wrinkle recovery. Formaldehyde release less than 10ppm was obtained only by non-formaldehyde resin. Considering other factors, the optimal concentration of non-formaldehyde resin was shown to be 9-11%. In case of low-formaldehyde type, 5-7%resin concentration and curing temperature of 160~170℃ were recommended for optimal finishing condition. The choice and combination of resins and catalysts were also important factors, and preliminary considerations before treating cotton fabrics with resins used in this study are also important to get much better results.
KW - non-formaldehyde resin;low-formaldehyde resin;formaldehyde release;tear strength;shrinkage;wrinkle recovery;DP finishing
DO - 10.5764/TCF.2012.24.2.121
ER -
김한기, Namsik Yoon, Manwoo Huh and 김익수. (2012). Physicochemical Properties of Non-Formaldehyde Resin Finished Cotton Fabric and their Optimal Treatment Condition. Textile Coloration and Finishing , 24(2), 121-130.
김한기, Namsik Yoon, Manwoo Huh and 김익수. 2012, "Physicochemical Properties of Non-Formaldehyde Resin Finished Cotton Fabric and their Optimal Treatment Condition", Textile Coloration and Finishing , vol.24, no.2 pp.121-130. Available from: doi:10.5764/TCF.2012.24.2.121
김한기, Namsik Yoon, Manwoo Huh, 김익수 "Physicochemical Properties of Non-Formaldehyde Resin Finished Cotton Fabric and their Optimal Treatment Condition" Textile Coloration and Finishing 24.2 pp.121-130 (2012) : 121.
김한기, Namsik Yoon, Manwoo Huh, 김익수. Physicochemical Properties of Non-Formaldehyde Resin Finished Cotton Fabric and their Optimal Treatment Condition. 2012; 24(2), 121-130. Available from: doi:10.5764/TCF.2012.24.2.121
김한기, Namsik Yoon, Manwoo Huh and 김익수. "Physicochemical Properties of Non-Formaldehyde Resin Finished Cotton Fabric and their Optimal Treatment Condition" Textile Coloration and Finishing 24, no.2 (2012) : 121-130.doi: 10.5764/TCF.2012.24.2.121
김한기; Namsik Yoon; Manwoo Huh; 김익수. Physicochemical Properties of Non-Formaldehyde Resin Finished Cotton Fabric and their Optimal Treatment Condition. Textile Coloration and Finishing , 24(2), 121-130. doi: 10.5764/TCF.2012.24.2.121
김한기; Namsik Yoon; Manwoo Huh; 김익수. Physicochemical Properties of Non-Formaldehyde Resin Finished Cotton Fabric and their Optimal Treatment Condition. Textile Coloration and Finishing . 2012; 24(2) 121-130. doi: 10.5764/TCF.2012.24.2.121
김한기, Namsik Yoon, Manwoo Huh, 김익수. Physicochemical Properties of Non-Formaldehyde Resin Finished Cotton Fabric and their Optimal Treatment Condition. 2012; 24(2), 121-130. Available from: doi:10.5764/TCF.2012.24.2.121
김한기, Namsik Yoon, Manwoo Huh and 김익수. "Physicochemical Properties of Non-Formaldehyde Resin Finished Cotton Fabric and their Optimal Treatment Condition" Textile Coloration and Finishing 24, no.2 (2012) : 121-130.doi: 10.5764/TCF.2012.24.2.121