본문 바로가기
  • Home

Microstructure and mechanical properties of B4C-SiC composites

  • Journal of the Korean Crystal Growth and Crystal Technology
  • Abbr : J. Korean Cryst. Growth Cryst. Technol.
  • 2019, 29(6), pp.338~344
  • DOI : 10.6111/JKCGCT.2019.29.6.338
  • Publisher : The Korea Association Of Crystal Growth, Inc.
  • Research Area : Engineering > Materials Science and Engineering
  • Received : November 19, 2019
  • Accepted : December 12, 2019
  • Published : December 31, 2019

Seong Min So 1,  Kyounghun Kim 1,  Park Joo-Soek 1,  Min Suk Kim 2,  HyungSun Kim 3

1한국세라믹기술원
2인하대학교 신소재공학과
3인하대학교

Accredited

ABSTRACT

B4C-SiC composites were fabricated using hot press sintering method without sintering additives at 1,900~2,000° Cunder a pressure of 40 MPa. The crystal phase, relative density, microstructure, and mechanical properties of B4C-SiC composites were evaluated. When B4C and SiC were uniformly dispersed in the composite, grain growth was inhibited, and a sintered body with a fine and uniform microstructure, with improved mechanical properties, was fabricated. The relative density of B4C-SiC composites sintered under 2,000°C of temperature and 40 MPa of pressure was over 99.8 %, and the bending strength and Vicker’s hardness at 50 wt% of B4C were 645 MPa and 30.6 GPa, respectively.

Journal Copyright Policy

BY-NC 아이콘

This license enables reusers to distribute, remix, adapt, and build upon the material in any medium or format for noncommercial purposes only, and only so long as attribution is given to the creator.

Citation status

* References for papers published after 2025 are currently being built.