Optical properties of (CexLu1 − x)3MgAl3SiO12 yellow phosphor

  • Journal of the Korean Crystal Growth and Crystal Technology
  • Abbr : J. Korean Cryst. Growth Cryst. Technol.
  • 2016, 26(1), pp.14-18
  • DOI : 10.6111/JKCGCT.2016.26.1.014
  • Publisher : The Korea Association Of Crystal Growth, Inc.
  • Research Area : Engineering > Materials Science and Engineering
  • Published : February 29, 2016

Jung-Il Lee 1 Tae Wan Kim 1 Ho Ra Oh 1 Hong, Chang-woo 1 Jeong-ho Ryu 1

1한국교통대학교

Accredited

ABSTRACT

A novel Ce3+ doped (CexLu1 − x)3MgAl3SiO12 phosphor was successfully synthesized by a conventional solid-state reaction. Heat-treatment temperature was controlled from 1250 to 1550oC for 5 h. XRD and PL properties were analyzed for the optimum heat-treatment condition. Ce doping concentration was varied from 2.0 to 10.0 mol% for the optimum Ce doping concentration. The PL intensity, peak wavelength and FWHM were calculated with the Ce doping concentration, and evaluated for the application to LED packaging. Particle size and morphology were also characterized for synthesized phosphor sample at optimum heat-temperature and Ce doping concentration.